Supply Inconel, Monel, Cobalt & Beryllium Alloys

offer an Extensive Range of Material Grades

Super Alloy materials, including Inconel, Monel, Hastelloy, Cobalt, Beryllium alloys, exhibit extraordinary properties: high strength, high wear resistance, high-temp stability or extreme corrosion resistance, and are mainly used in critical operating environments in petrochemical, marine and power plant industries. Click here to find essential knowledge about superalloys.

Hastelloy

C22, C276

Inconel

Inconel 600, Inconel 625, Inconel 718

Incoloy

Alloy 20, Incoloy 800/800H, Incoloy 825

Cobalt Alloy

Stellite 3
Stelite 6B

Monel

Monel 400

Beryllium Cooper

CDA172

Offer Raw Materials, Fasteners, Fully Machined, or Welding Consumables

We provide an extensive selection of super alloy products, available in various forms including Bars, Plates, Fasteners, Pipes, Fittings, Flanges, as well as Machined Parts and Welding Consumables.

Inconel, Monel, Beryllium Bar
Bar
Inconel fastener
Fastener
Inconel, Hastelloy, Monel, Stellite, Cobalt, Beryllium
Welding Electrode
 Inconel, Monel, Beryllium Pipe
Nickel alloy
Pipe
Nickel alloy
Inconel
Fitting
Inconel, Hastelloy, Monel, Stellite,
Nickel Alloy
Machined Samples
Inconel, Monel, Cobalt and Stellite
Nickel alloy

Our Key Advantages

  • Strategic partnership with tier one mills
  • Capable of supplying raw materials or fully machined parts
  • Accommodate low volume order
  • Short Lead Time
  • Door to Door logistic service
Superalloys + Machining
Accept Low Qty Order
Short Lead Time

Manufacturing Process of Inconel & Monel

Beryllium cooper
Nickel alloy
Inconel
Vacuum Melting
Inconel, Monel and Cobalt electro slag remelting
Electro Slag Remelting
Inconel
Nickel Alloy
Inconel Fastener
Forging
Inconel, Monel, Cobalt, Stellite
Beryllium Cooper
Nickel Alloy
Heat Treatment

Process Inspection & Cert of Inconel, Monel …

Process

We implement state of art melting process: Vacuum Melting -> ESR -> Forging -> Heat Treatment -> Machining.

Inspection

We conduct chemical composition inspection, mechanical properties test and other NDTs (PT and UT) for each heat log.

Material Cert

We issue material certification per EN10204 Type 3.1

Quality Certification

ISO9001 ISO14001 Certification
ISO9001, ISO14001
ISO17025 ISO45001 Certification
ISO45001, ISO17025
CE PED, NORSOK M650 Certification
CE PED, NORSOK M650
API-20A API-20B Certification
API-20A, API-20B

Material Specification

Hastelloy C22 and C276 

     These alloys exhibit excellent resistance to both oxidizing and reducing acid environments, as well as those containing mixed acids. It is particularly useful for resistance to pitting and crevice corrosion in acid-halide environments. The low carbon content minimizes carbide precipitation during welding to maintain corrosion resistance in as-welded structures.

Chemical Composition
Grade SymbalUNS DesignationCarbonManganesePhosphorusSulfurSiliconChromiumNickelMolybdenumOthers
Hastelloy C22UNS N060220.0150.50.020.020.0820.0-22.5Balance12.5-14.5Thungsten 2.5-3.0; Cobalt 2.5; Vanadium 0.35;
Hastelloy C276UNS N102760.0110.040.040.0814.5-16.5Balance15.0-17.0Iron 4.0-7.0; Tungsten 3.0-4.5; Cobalt 2.5; Vandium 0.35;
Mechanical Properities and ASTM Specifications
Grade SymbalUNS DesignationConditionTensile StrengthTensile StrengthYield StegnthYield StrengthElongation in 2in or 4D min%PipePipeSheetBarForgingFitting
min ksimin MPamin ksimin MPaSmlsPlate
Hastelloy C22UNS N06022Solution Annealed1006904531045B622B619B575B574B564B366
Hastelloy C276UNS N10276Solution Annealed1006904128340B622B575B574B564B366
Inconel 600, 625 and 718 

     These high strength alloys are designed to resist a wide range of severely corrosive environments, pitting and crevice corrosion.

Chemical Composition
Grade SymbalUNS DesignationCarbonManganesePhosphorusSulfurSiliconChromiumNickelMolybdenumOthers
Inconel 600UNS N066000.1510.0150.514.0-17.072.0 minCu 0.5; Iron 6.0-10.0
Inconel 625UNS N066250.10.0350.0150.0150.520.0-23.058.0 min8.0-10.0Fe 5.0; Cobalt 1.0 max; Columbium+Tantalum 3.15-4.15; Al 0.40 max; Ti 0.40 max;
Inconel 718UNS N077180.080.0350.0150.0150.03517.0-21.050.0-55.02.8-3.3Cu 0.3; Boron 0.006 max; Columbium+Tantalum 4.75-5.50; Ti 0.65-1.15; Cobalt 1.0 max
Mechanical Properities and ASTM Specifications
Grade SymbalUNS DesignationConditionTensile StrengthTensile StrengthYield StegnthYield StrengthElongation in 2in or 4D min%Reduction of Area, C, D min%Brinell Hardness, HBWPipeBarForgingFitting
min ksimin MPamin ksimin MPa
Inconel 600UNS N06600Annealed805523524130B167B166B564B366
Inconel 625UNS N06625Annealed1206030B444B446
Inconel 718UNS N07718Solution + Precipitation harden185127515010341215331 minB637
Incoloy 800/800H, 825 and Alloy 20

     These nickel steel alloys are designed to provide exceptional resistance to many corrosive environments. They have excellent resistance to both reducing and oxidizing acids, to stress-corrosion cracking, and to localized attack such as pitting and crevice corrosion.

Chemical Composition
Grade SymbalUNS DesignationCarbonManganesePhosphorusSulfurSiliconChromiumNickelMolybdenumOthers
Incoloy 800UNS N088000.11.50.0450.015119.0-23.030.0-35.0Fe 39.5 min; Cu 0.75; Al 0.15-0.60; Ti 0.15-0.60;
Incoloy 800HUNS N088100.11.50.0450.015119.0-23.030.0-35.0Fe 39.5 min; Cu 0.75; Al 0.15-0.60; Ti 0.15-0.60;
Incoloy 825UNS NO88250.0510.030.519.5-23.538.0-46.02.5-3.5Fe 22.0 min; Cu 1.5-3.0; Ti 0.6-1.2; Al 0.2;
Alloy 20UNS N080200.0720.0450.03119.0-21.032.0-38.02.0-3.0Cu 3.0-4.0; Nb 8 x C min 1.00 max;
Mechanical Properities and ASTM Specifications
Grade SymbalUNS DesignationConditionTensile StrengthTensile StrengthYield StegnthYield StrengthElongation in 2in or 4D min%Reduction of Area, C, D min%Brinell Hardness, HBWPipeBarForgingFitting
min ksimin MPamin ksimin MPa
Incoloy 800UNS N08800Annealed755153020530192B407B408B564B366
Incoloy 800HUNS N08810Annealed654402517030192B407B408B564B366
Incoloy 825UNS N08825Annealed855863524030B423B425B564B366
Alloy 20UNS N08020Solution Annealed80550352403050B729B473B462B366
Monel 400

     This nickel alloy exhibits characteristics like good corrosion resistance, good weldability and high strength. A low corrosion rate in rapidly flowing brackish or seawater combined with excellent resistance to stress-corrosion cracking in most freshwaters, and its resistance to a variety of corrosive conditions led to its wide use in marine applications and other non-oxidizing chloride solutions.

Chemical Composition
Grade SymbalUNS DesignationCarbonManganesePhosphorusSulfurSiliconChromiumNickelMolybdenumOthers
Monel 400UNS N044000.320.0240.563.0 minCu 28.0-34.0; Fe 2.5 max;
Mechanical Properities and ASTM Specifications
Grade SymbalUNS DesignationConditionTensile StrengthTensile StrengthYield StegnthYield StrengthElongation in 2in or 4D min%Reduction of Area, C, D min%PipeBarForgingFitting
min ksimin MPamin ksimin MPa
Monel 400UNS N04400Annealed704832517235B165B164B564B366
Stellite 6B

     This Cobalt Alloy is used in applications where wear, corrosion and high temperature resistance are needed. It is most commonly found in directional drilling tools, aerospace applications, valve parts, shaft sleeves and tools.

Chemical Composition
Grade SymbalUNS DesignationCarbonManganesePhosphorusSulfurSiliconChromiumNickelMolybdenumOthers
Stellite 6BUNS R300160.9-1.420.040.03228-3231.5Tungsten 3.5-5.5; Fe 3.0 max; Cobalt balance
Mechanical Properities and ASTM Specifications
Grade SymbalUNS DesignationConditionTensile StrengthTensile StrengthYield StegnthYield StrengthElongation in 2in or 4D min%Reduction of Area, C, D min%BarPlate
min ksimin MPamin ksimin MPa
Stellite 6BUNS R30016Solution15410639363857AMS 5894AMS 5894

CDA172

Beryllium Copper is notable for its highest strength and hardness compared to commercial copper alloys.

Chemical Composition
Grade SymbalUNS DesignationBeCoCuSiFeAlOthers
CDA172UNS C172001.8-2.0> 0.2Remaining0.150.150.2
Mechanical Properities and ASTM Specifications
Grade SymbalUNS DesignationConditionTensile StrengthTensile StrengthYield StegnthYield StrengthElongation in 2in or 4D min%Reduction of Area, C, D min%Hardness
min ksimin MPamin ksimin MPa
CDA172UNS C17200Solution + Precipitation1651137140965336-45 HRC

Inconel, Incoloy and Monel are trademarks of Special Metals Corporation, Stellite is a trademark of Kennametal Inc., and Hastelloy is a trademark of Haynes International Inc. We offer equivalent products.

Email us

sales@sintermatic.com

Address

17890 Castleton Ste.398 Rowland Height, CA91748 US

We Believe Quality is Everything!